The largest peak shear resistance does not necessarily identify the interface that retains the most resistance after sliding. A new peer-reviewed paper by Mohammad Mehdi Haj Ghanbari, Mohammad Mohsen Toufigh and Vahid Toufigh examines that distinction through direct-shear tests and multi-criteria analysis. Published online on 10 November 2026 in the Journal of Infrastructure Preservation and Resilience, it remains an accepted Article in Press. This review draws on the full 22-page manuscript and its supplement; Civil Insight’s analysis has not itself undergone peer review.

The experimental comparison
The researchers tested two granular soils from the Ekhtiyar-Abad area of Kerman, Iran: a poorly graded sand, classified SP, and a well-graded sand with silt, SW–SM. They compared dry specimens with specimens at Standard Proctor optimum moisture content, using 100 × 100 mm and 300 × 300 mm shear boxes. Normal stresses were 50, 100 and 200 kPa, with each condition reported as tested in triplicate.
Four configurations formed the main comparison: an unreinforced reference, an HDPE geogrid, a carbon-fibre-reinforced polymer sheet and epoxy-impregnated CFRP. For interface tests, the reinforcement was bonded to a rigid steel backing at the prescribed shear plane. The CFRP fibre direction and geogrid orientation were fixed. These are controlled interface tests, rather than full reinforced-soil walls or pullout tests.
Shearing proceeded at 1 mm/min, with the common response indices evaluated to 10 mm horizontal displacement. A further epoxy-only control series in the larger box helped examine whether the combined fibre–resin response could be explained by resin alone.

What the measurements show
One comparison illustrates the importance of scope. For SW–SM at optimum moisture content, in the 300 mm box under 200 kPa normal stress, reported peak shear stresses were 127.8 kPa for the reference, 141.9 kPa for geogrid and 143.6 kPa for epoxy-impregnated CFRP. The latter two values were 11.03% and 12.36% above their matched reference. They are results for that condition, not general improvement factors for site design.
Across the programme, the authors associated geogrid performance with interlocking and dilation, while CFRP-based interfaces showed stronger post-peak retention. The epoxy-modified response was consistent with an adhesion-related contribution, but bond strength and microstructural mechanisms were not directly measured. The epoxy-only control supported a combined fibre–resin contribution rather than attributing the result to resin alone.
A ranking that changes with the question
The decision analysis combined six measures: peak resistance, resistance at large displacement, an initial stiffness index, post-peak retention, displacement to peak and an interface shear-work index. The large-displacement measure was the mean stress between 9 and 10 mm. A true residual-strength plateau was not demonstrated. Likewise, the area under the curve to 10 mm is shear work per unit interface area, not a measurement of material fracture toughness.
TOPSIS ranks alternatives by their distance from ideal and least-desirable combinations of the chosen measures. The baseline scores placed epoxy-impregnated CFRP first at 0.680 and geogrid second at 0.661. These dimensionless scores depend on the selected criteria and weights; they are not safety factors or probabilities of success.
The authors then varied the weight assigned to the larger box, the combination of weighting methods, and whether displacement to peak was beneficial, undesirable or excluded. Across 45 scenarios, geogrid ranked first 24 times and epoxy-impregnated CFRP 21 times. Both remained in the leading pair. The robust finding is their separation from the other alternatives within this analysis, while their order remains sensitive to the engineering question.
Where confidence and transferability stop
Civil Insight’s assessment: matched test conditions, triplicate runs and explicit sensitivity checks are strengths. However, only three normal-stress levels underpin each fitted strength envelope. Very high regression fit values therefore do not establish precisely known friction angles or apparent cohesion; the supplement reports wide confidence intervals.
The intended drained condition was not verified by pore-water-pressure measurements. Optimum-moisture tests should not be treated as saturated or suction-controlled tests. The paper also acknowledges uncertainty from the stress-area basis at large displacement. A 300 mm box reduces some boundary effects, but does not establish field-scale behaviour.
The supplement provides regression diagnostics and decision matrices, not raw replicate histories. The manuscript’s statement that no datasets were generated or analysed is difficult to reconcile with its experimental account, limiting independent checking. Cyclic loading, long-term environmental exposure, other reinforcement orientations and full-scale validation remain outside the demonstrated scope.
Implications for practice
For Australian retaining-wall and earthworks teams, the useful lesson is to define the required interface behaviour before comparing headline strengths. Peak resistance, movement to mobilise it and resistance after movement answer different design questions. The study supports more informed review of laboratory evidence; it does not establish an interchangeable CFRP replacement for a specified geogrid or provide project-ready Australian design parameters.
Original paper and image credits
Haj Ghanbari, M.M.; Toufigh, M.M.; Toufigh, V. (2026). Multi-criteria experimental evaluation of soil–reinforcement interface systems under direct shear loading. Journal of Infrastructure Preservation and Resilience. Published 10 November 2026; peer-reviewed accepted Article in Press. DOI: 10.1186/s43065-026-00223-w. Full accepted manuscript and supplement. No linked correction or retraction was located in publisher, DOI-record and search checks on 23 November 2026.
Featured specimen-preparation and interface photographs: Figure 3; supporting laboratory apparatus photographs: Figure 2. © Haj Ghanbari, Toufigh and Toufigh (2026), CC BY 4.0. Both figures document the reviewed study.